Packaging (forming, sealing, wrapping, case packing, palletizing)
Heat sealing in intermittent-motion form-fill-seal packaging
In short
Packaging (forming, sealing, wrapping, case packing, palletizing) can use at most 99 of every 100 planned hours. The rest goes to limits no plant can avoid.
- 99usable at most
- 1are a physical limit
The three limits that set it
Running time: up to 100 %
The rest are stops imposed by physics or by regulation: cleaning, changeovers, defrosting.
Speed: up to 99 %
How close to its maximum speed it can run without damaging the product or the equipment.
Good product: up to 100 %
Some product falls outside specification even with the process well under control.
Technical detail
Uncertainty intervals, physical models per station and sources, for anyone who wants to check each figure.
1Scenario
A vertical form-fill-seal machine forms pillow bags of frozen vegetables or a similar dry product from a reel of polyethylene film. Each cycle the film is advanced by one bag length, the cross-sealing jaws close on two layers of film, hold them at constant jaw temperature for the dwell time (the top seal of one bag and the bottom seal of the next are made together) and open again. The longitudinal fin seal is made while the film advances. The cross-seal dwell is the physics-limited step.
2Results
- Density of the semicrystalline sealant film (two-phase rule)914 [900–928] kg/m³
- Specific heat of the semicrystalline film (crystalline and amorphous heat capacities weighted by crystallinity)1.95 [1.89–2.01] kJ/kg/K
- Thermal diffusivity of the film0.186 [0.143–0.250] mm²/s
- Fourier number at which the seal interface reaches the sealing temperature0.676 [0.584–0.819]
- TheoreticalMinimum jaw dwell time (interface reaches the sealing temperature, ideal contact)0.00911 [0.00405–0.02034] s
- Dwell time with the capability margin (jaw-temperature and film-thickness tolerances; declared tolerances, not a documented BAT)0.0146 [0.0064–0.0346] s
- TypicalDwell time in operation (declared scenario)0.300 [0.162–0.589] s
- Minimum indexing time per cycle (film advance and jaw stroke, bang-bang motion)0.370 [0.283–0.464] s
- TheoreticalMaximum cycles per minute with the minimum dwell158 [126–205] 1/min
- Cycles per minute with the capability-limited dwell (the rate of the capable process)156 [125–202] 1/min
- TypicalCycles per minute with the operating dwell (declared scenario)89.6 [61.2–122.7] 1/min
- Film mass in the seal areas per pack (two layers)0.393 [0.282–0.544] g
- TheoreticalThermodynamic minimum energy per pack (the seal returns to ambient)0 J
- Minimum heating duty per pack without heat recovery (seal mass at the sealing temperature, fusion included; a computed minimum, not a documented BAT)124 [87–182] J
- Heat absorbed per pack by the film at the capability-limited dwell (conductive jaws)141 [100–207] J
- TypicalHeat absorbed per pack by the film at the operating dwell (film close to jaw temperature)147 [104–214] J
- Minimum sealing heat per kg of packed product0.247 [0.175–0.365] kJ/kg
- Sealing heat absorbed by the film per kg of packed product at the operating dwell0.293 [0.207–0.429] kJ/kg
- Nominal interface temperature at the capability-limited dwell139 [126–152] °C
- Standard deviation of the interface temperature at the capability-limited dwell4.01 [2.77–5.59] K
- Share of seals whose interface stays below the sealing temperature9.75 × 10⁻⁷ [4.14 × 10⁻⁹–8.55 × 10⁻⁵]
- Share of seals overheated beyond the upper limit of the sealing window7.62 × 10⁻²⁴ [1.87 × 10⁻¹²⁰–1.10 × 10⁻⁶]
- TheoreticalMaximum OEE quality factor (seal integrity)1.00000 [0.99990–1.00000]
- Mean film speed at the capability-limited rate39.0 [31.1–50.4] m/min
- Run time of one reel at the capability-limited rate51.2 [25.6–109.0] min
- TheoreticalMaximum film yield (splice and start-up waste)0.9982 [0.9955–0.9994]
- TheoreticalMaximum availability (no stop is forced by physics or regulation: reel splices are removable by an automatic splicer, changeovers are scenario)1.00
- Availability with declared manual splices and changeovers0.909 [0.815–0.963]
- TheoreticalPerformance factor: minimum cycle over capability-limited cycle0.986 [0.959–0.995]
- TheoreticalPhysics-bounded OEE0.986 [0.959–0.995]
- OEE with declared manual splices and changeovers0.896 [0.799–0.950]
3Ceilings per dimension
- Theoretical
- Best available technique
- Best documented
- Typical
- TheoreticalMinimum jaw dwell time (interface reaches the sealing temperature, ideal contact)0.00911 [0.00405–0.02034] s
- TypicalDwell time in operation (declared scenario)0.300 [0.162–0.589] s
- TheoreticalMaximum cycles per minute with the minimum dwell158 [126–205] 1/min
- TypicalCycles per minute with the operating dwell (declared scenario)89.6 [61.2–122.7] 1/min
- TheoreticalThermodynamic minimum energy per pack (the seal returns to ambient)0 J
- TypicalHeat absorbed per pack by the film at the operating dwell (film close to jaw temperature)147 [104–214] J
- TheoreticalMaximum OEE quality factor (seal integrity)1.00000 [0.99990–1.00000]
- TheoreticalMaximum film yield (splice and start-up waste)0.9982 [0.9955–0.9994]
- TheoreticalMaximum availability (no stop is forced by physics or regulation: reel splices are removable by an automatic splicer, changeovers are scenario)1.00
- TheoreticalPerformance factor: minimum cycle over capability-limited cycle0.986 [0.959–0.995]
- TheoreticalPhysics-bounded OEE0.986 [0.959–0.995]
4Loss cascade
- TheoreticalTypicalCycle or residence time0.00911 [0.00405–0.02034] s → 0.300 [0.162–0.589] s (gap 0.291 s)
The minimum dwell brings the nominal seal interface exactly to the sealing temperature with ideal (zero-resistance) contact between jaw and film. Any real jaw temperature oscillates around its set point and the film thickness varies along the web, so a capable process must hold the jaws until the interface is z standard deviations of jaw temperature above the sealing temperature on the thickest film of the tolerance band. Because the remaining temperature difference decays exponentially with the Fourier number, the last few kelvin cost a disproportionate share of the dwell. Operating dwells are one or two orders of magnitude longer than the conduction limit of a bare polyethylene film. The causes are thermal resistances that the ideal model leaves out: non-stick jaw covers, imperfect contact on wrinkles and fin overlaps, outer laminate layers (oriented polypropylene or polyester) that must be crossed before the sealant, the latent heat of melting that slows the advance of the melt front, and the time the molten interface needs for chain interdiffusion and for the seal to gain strength while still under pressure.
- TheoreticalTypicalThroughput158 [126–205] 1/min → 89.6 [61.2–122.7] 1/min (gap 68.8 1/min)
With the indexing motion (film advance and jaw stroke) fixed by the acceleration the film and the carriage can stand, the cycle rate falls from the theoretical value (minimum dwell) to the capable value and then to the operating value in proportion to the dwell gaps above; at operating dwells the dwell, not the motion, dominates the cycle.
- TheoreticalTypicalEnergy per unit of product0 J → 147 [104–214] J (gap 147 J)
The seal is heated and cools back to ambient, so in the reversible limit (ideal heat recovery) no net energy is needed: the thermodynamic minimum is zero, as in the DOE bandwidth study. Without heat recovery the least heat is that of raising only the seal mass to the sealing temperature and melting its crystalline fraction. Conductive jaws at a constant temperature above the sealing temperature heat the whole film thickness towards the jaw temperature; at operating dwells the film reaches it, so the absorbed heat grows with (T_jaw - T0) instead of (T_s - T0). The heat absorbed by the film is still a small fraction of the electricity of the machine: jaw heaters lose heat continuously by convection and radiation and through the jaw mountings, and the drives, vacuum and compressed air dominate the energy of a packaging step, which is why the documented energy intensities of packaging are orders of magnitude above the sealing heat.
5Physics-bounded OEE
- Loading time (ideal)1.000
- Availabilityfactor 1.001.000 (−0.000)
- Performancefactor 0.986 [0.959–0.995]0.986 (−0.014)
- Qualityfactor 1.00000 [0.99990–1.00000]0.986 (−0.000)
- Physics-bounded OEE0.986 [0.959–0.995]
6Full derivation
Scope. An intermittent-motion vertical form-fill-seal machine makes pillow bags from a reel of polyethylene film. Each cycle the film advances one bag length, the cross-sealing jaws close on two film layers, hold them at a constant jaw temperature for the dwell time and open again; the longitudinal fin seal is made while the film moves. The cross-seal dwell is the physics-limited step. Symbols and their values, units, uncertainty distributions and sources are listed in the parameter table generated from config/physics/packaging.yaml. Numbers quoted here are point values; the output table gives the Monte Carlo intervals.
1. Mass balance — maximum film yield
Sealing consumes no product and no film: the seal is part of the bag. Film is lost only where it does not become a saleable bag. In a fin-sealed pillow bag there is no trim, so two losses remain:
- Splice waste. A reel holds a finite length . When it runs out the new web is spliced to the old one and a length around the splice is discarded.
- Start-up waste. After each changeover the machine needs bags to stabilise registration, bag length and seal quality.
During a production campaign of duration at web speed the film used for good bags is , the number of reels is , and
where is the film length per bag. No open source documents splice or start-up waste, so and are declared scenario values.
2. Energy balance — minimum energy per pack
Film properties. The sealant is semicrystalline polyethylene with mass crystallinity . Its density follows the two-phase rule from the densities of the crystalline and amorphous phases at 298 K ( = 1.0030 and = 0.8519 Mg/m³, Gaur and Wunderlich, 1981):
The specific heat weights the recommended heat capacities of crystalline and amorphous polyethylene at 310 K ( = 22.38 and = 31.33 J/(mol K) per CH2 repeat unit, = 14.027 g/mol):
Heat capacity rises with temperature, so using the 310 K value over the whole heating range underestimates the sensible heat: every energy computed with it is a lower bound. Melting the crystalline fraction absorbs , with the heat of fusion of fully crystalline polyethylene = 4.051 kJ/mol at 380 K.
Seal mass. The cross seal covers the bag width times the jaw height (the top seal of one bag and the bottom seal of the next), the fin seal the bag length times the fin width ; both join two layers of thickness :
Thermodynamic minimum. The seal is heated, fused and cooled back to ambient: its final state equals its initial state except for the new bond, whose interfacial energy is negligible. In the reversible limit all the heat could be recovered (ideal regeneration), so the thermodynamic minimum is zero, in agreement with the zero thermodynamic minimum the DOE bandwidth study assigns to packaging.
Minimum heating duty without recovery. Without heat recovery, the least heat is that of bringing the seal mass to the sealing temperature and melting its crystalline fraction. Heat flows from the jaw to the interface, so when the interface reaches every point between jaw and interface is at least at ; uniform heating to is therefore the lowest possible duty:
Conductive jaws. A jaw held at heats the film towards . The heat absorbed after a dwell follows from the mean temperature of the plane wall (Section 3):
141 J at the capability-limited dwell and 147 J at the operating dwell, where the film is practically at jaw temperature. Per kilogram of product (0.5 kg bags) the sealing heat is 0.25–0.29 kJ/kg, two orders of magnitude below the documented energy intensity of a whole packaging step (DOE, frozen vegetables: 14 Btu/lb state of the art, 15 Btu/lb typical, i.e. 33–35 kJ/kg). The rest is machinery: jaw heaters losing heat continuously by convection and radiation, drives, vacuum and compressed air.
3. Rate-limiting step — minimum dwell and maximum cycle rate
Heat conduction problem. The two film layers form a slab of thickness whose two faces are suddenly brought to when the jaws close; the seal interface is the mid-plane. With ideal contact (no thermal resistance between jaw and film) and constant properties, the temperature obeys the one-dimensional heat equation , with the thermal diffusivity
where is the thermal conductivity of the film. No open source with a quotable conductivity of polyethylene film was found, so is a declared scenario value (0.33 W/(m K), range 0.25–0.45). The classical separation-of-variables solution for the plane wall of half-thickness gives the dimensionless mid-plane temperature
and the dimensionless mean temperature
, the Fourier number, compares the dwell with the time heat needs to diffuse across one film layer. For the first term alone is accurate to better than 0.2%.
Minimum dwell. The seal is sound when the interface reaches , i.e. when . Solving (bisection on the series):
With K = 150 °C, = 25 °C and = 50 µm, = 0.24, = 0.676 and = 9.1 ms. The dwell scales with and with : doubling the film thickness quadruples it. The latent heat of melting is left out of the conduction problem; it slows the advance of the melt front, so is a lower bound.
Capability-limited dwell. The jaw temperature fluctuates with standard deviation and the film thickness with coefficient of variation . A capable process holds the jaws until the interface is above on the thickest film of the tolerance band, :
Indexing motion. Between two seals the film advances one bag length and each jaw travels its stroke open and closed. The fastest motion over a distance with a maximum acceleration is bang-bang (accelerate half-way, decelerate half-way), lasting :
Cycle rates.
where = 0.30 s is the dwell set in operation (declared scenario). Operating dwells are one to two orders of magnitude above the conduction limit of a bare film because of jaw covers, contact resistance, outer laminate layers, latent heat and the time the molten interface needs for chain interdiffusion; these are explained in the loss cascade.
4. Process capability — quality ceiling
At the capability-limited dwell the interface temperature depends on the jaw temperature and on the film thickness. A first-order propagation of their variability gives
with the derivatives evaluated numerically on the conduction solution. Two defects are counted:
where is the nominal interface temperature (139 °C), the width of the sealing window above (beyond it the film thins, shrinks or burns through) and the standard normal distribution function. Then
With a 3σ margin the under-seal share is about ; the quality ceiling falls when the jaw set point approaches the upper limit of the window.
5. Unavoidable stops — maximum availability
A reel lasts = 51 min at the capability-limited web speed = 39 m/min. Each manual reel change stops the machine for , but an automatic zero-speed splicer removes the stop (not the splice waste), and each campaign ends with a changeover of duration , a decision of the product mix. Neither stop is forced by physics or regulation, and no cleaning-in-place applies to the machine (the cleaning model is not used), so
With the declared manual splices and changeovers,
which enters only oee_scenario.
6. Physics-bounded OEE
Scope of the bound. The theoretical label of means physics-bounded under the declared scenario: the ceiling follows from the physics of the operation for the declared product, equipment and schedule, and it is a bound only conditional on those declarations. It follows the common definition of all models: counts only stops required by regulation or forced by a physical mechanism, at their physical minimum duration, plus the start-up they force; is the ratio of the physics-limited ideal cycle to the cycle of the capable process; is the share of conforming units, and mass losses of conforming product are reported only as yield.
The performance ceiling compares the capability-limited cycle with the pure conduction limit: it is the price of making every seal sound. The result is = 0.986, set by the seal capability margin; with the declared manual splices and changeovers, oee_scenario = 0.896. The capability-limited dwell and rate use declared tolerances, so they are reported without the best-available-technique label.
7. Assumptions and validity
See the assumption and validity lists generated from the configuration file. The most influential inputs (sensitivity table) are the splice and changeover durations, the reel length and the campaign length for OEE; the film thickness, conductivity and jaw-to-seal temperature difference for the dwell.
References
- Gaur, U., Wunderlich, B. (1981). Heat capacity and other thermodynamic properties of linear macromolecules. II. Polyethylene. Journal of Physical and Chemical Reference Data, 10, 119–152. doi:10.1063/1.555636
- U.S. Department of Energy. Bandwidth Study on Energy Use and Potential Energy Saving Opportunities in U.S. Food and Beverage Manufacturing, 2017.
7Parameters and provenance
- 0.45
Mass-fraction crystallinity of the polyethylene sealant film
Scenario · Uniform 0.35 to 0.55
Declared assumptionRange of low-density polyethylene films; declared assumption.
- 1.003 Mg/m³
Density of crystalline polyethylene at 298 K
Property · Fixed
Verified quoteShow verbatim quote
recalculated using eq (2) and p,. = 1.0030 Mg mHeat capacity and other thermodynamic properties of linear macromolecules. II. Polyethylene (Gaur, U.; Wunderlich, B.), Journal of Physical and Chemical Reference Data 10, 119 (1981) (opens in a new tab). American Institute of Physics for the National Institute of Standards and Technology (NIST reprint), 1981. p. 5. doi:10.1063/1.555636
- 0.8519 Mg/m³
Density of amorphous polyethylene at 298 K
Property · Fixed
Verified quoteShow verbatim quote
The amorphous density has been well established at 0.8519Heat capacity and other thermodynamic properties of linear macromolecules. II. Polyethylene (Gaur, U.; Wunderlich, B.), Journal of Physical and Chemical Reference Data 10, 119 (1981) (opens in a new tab). American Institute of Physics for the National Institute of Standards and Technology (NIST reprint), 1981. p. 4. doi:10.1063/1.555636
- 22.38 J/mol/K
Heat capacity of crystalline polyethylene at 310 K, per mole of CH2 repeat unit (recommended data)
Property · Fixed
Verified quoteShow verbatim quote
310.0 22.38 3796Heat capacity and other thermodynamic properties of linear macromolecules. II. Polyethylene (Gaur, U.; Wunderlich, B.), Journal of Physical and Chemical Reference Data 10, 119 (1981) (opens in a new tab). American Institute of Physics for the National Institute of Standards and Technology (NIST reprint), 1981. p. 30. doi:10.1063/1.555636
- 31.33 J/mol/K
Heat capacity of amorphous polyethylene at 310 K, per mole of CH2 repeat unit (recommended data)
Property · Fixed
Verified quoteShow verbatim quote
310.0 31.33 4849.Heat capacity and other thermodynamic properties of linear macromolecules. II. Polyethylene (Gaur, U.; Wunderlich, B.), Journal of Physical and Chemical Reference Data 10, 119 (1981) (opens in a new tab). American Institute of Physics for the National Institute of Standards and Technology (NIST reprint), 1981. p. 26. doi:10.1063/1.555636
- 4.051 kJ/mol
Heat of fusion of fully crystalline polyethylene at 380 K, per mole of CH2
Property · Fixed
Verified quoteShow verbatim quote
380 4.051 390 4.084Heat capacity and other thermodynamic properties of linear macromolecules. II. Polyethylene (Gaur, U.; Wunderlich, B.), Journal of Physical and Chemical Reference Data 10, 119 (1981) (opens in a new tab). American Institute of Physics for the National Institute of Standards and Technology (NIST reprint), 1981. p. 32. doi:10.1063/1.555636
- 14.027 g/mol
Molar mass of the CH2 repeat unit
Property · Fixed
Computed12.011 + 2 x 1.008 g/mol (standard atomic weights).
- 0.33 W/m/K
Thermal conductivity of the polyethylene film
Scenario · Uniform 0.25 to 0.45 W/m/K
Declared assumptionNo open source with a quotable conductivity of polyethylene film was found; declared assumption with a wide range. It enters the dwell time inversely.
- 50 micrometer
Thickness of one film layer (distance from the jaw face to the seal interface)
Scenario · Uniform 35 to 70 micrometer
Declared assumption - 0.05
Coefficient of variation of the film thickness
Scenario · Uniform 0.03 to 0.08
Declared assumption - 25 °C
Initial film temperature
Scenario · Uniform 15 to 30 °C
Declared assumption - 120 °C
Interface temperature required for a sound seal (seal initiation temperature of the sealant)
Scenario · Uniform 110 to 130 °C
Declared assumptionMust lie above the melting range of the crystallites and below the equilibrium melting temperature of polyethylene (414.6 K); no open source with a quotable seal initiation temperature was used.
- 30 K
Jaw set-point above the sealing temperature
Scenario · Uniform 20 to 40 K
Declared assumption - 3 K
Standard deviation of the jaw face temperature under control
Scenario · Uniform 1.5 to 4 K
Declared assumption - 3
Capability margin in standard deviations used to set the capable dwell
Scenario · Uniform 2.5 to 3.5
Declared assumptionOperating choice, point value at the centre of the declared range 2.5-3.5; a larger margin lengthens the dwell and lowers the under-seal share.
- 60 K
Width of the sealing window above the sealing temperature (beyond it the film thins
Scenario · Uniform 50 to 70 K
Declared assumption - 0.3 s
Jaw dwell time set in operation (jaw covers, contact resistance and laminate layers lengthen it)
Scenario · Uniform 0.15 to 0.6 s
Declared assumptionNo open source with documented dwell times was used; declared assumption.
- 0.25 m
Film length per bag (index length)
Scenario · Fixed
Declared assumption - 0.15 m
Flat width of the bag (length of the cross seal)
Scenario · Fixed
Declared assumption - 0.012 m
Height of the cross-seal jaws (top seal of one bag plus bottom seal of the next)
Scenario · Fixed
Declared assumption - 0.01 m
Width of the longitudinal fin seal
Scenario · Fixed
Declared assumption - 0.5 kg
Mass of product per bag
Scenario · Fixed
Declared assumption - 20 m/s²
Maximum acceleration of the film transport (limited by film tension and slip of the pull belts)
Scenario · Uniform 10 to 40 m/s²
Declared assumption - 0.04 m
Opening stroke of each jaw
Scenario · Fixed
Declared assumption - 30 m/s²
Maximum acceleration of the jaw carriage
Scenario · Uniform 15 to 50 m/s²
Declared assumption - 2,000 m
Film length on one reel
Scenario · Uniform 1,000 to 4,000 m
Declared assumption - 3 m
Film wasted at each reel splice
Scenario · Uniform 1 to 6 m
Declared assumption - 3 min
Machine stop per manual reel change and splice (zero with an automatic zero-speed splicer)
Scenario · Uniform 1 to 6 min
Declared assumption - 8 h
Production time between two format or product changeovers
Scenario · Uniform 4 to 24 h
Declared assumption - 20 min
Duration of a changeover
Scenario · Uniform 10 to 45 min
Declared assumption - 20
Bags wasted while the machine stabilises after a changeover
Scenario · Uniform 5 to 50
Declared assumption
8Benchmarks
| Benchmark | Ceiling | Value | Provenance |
|---|---|---|---|
DOE bandwidth study, thermodynamic minimum energy intensity of packaging of frozen vegetablesShow verbatim quoteFreezing -53.5 to 586 279 279 -48.6 12.1 5.8 5.8 -1.02 Packaging 15 14 14 0Bandwidth Study on Energy Use and Potential Energy Savings Opportunities in U.S. Food and Beverage Manufacturing (opens in a new tab). U.S. Department of Energy, Office of Energy Efficiency and Renewable Energy, Advanced Manufacturing Office, 2017. p. 56. DOE/EE-1571; OSTI ID 1512366 | Theoretical | 0 Btu/lb | Verified quote |
DOE bandwidth study, state-of-the-art on-site energy intensity of packaging of frozen vegetables, per lb of product (whole packaging step; the theoretical output of this model is per pack, compare with heat_min_seal_per_kg)Show verbatim quoteFreezing -53.5 to 586 279 279 -48.6 12.1 5.8 5.8 -1.02 Packaging 15 14 14 0Bandwidth Study on Energy Use and Potential Energy Savings Opportunities in U.S. Food and Beverage Manufacturing (opens in a new tab). U.S. Department of Energy, Office of Energy Efficiency and Renewable Energy, Advanced Manufacturing Office, 2017. p. 56. DOE/EE-1571; OSTI ID 1512366 | Best available technique | 14 Btu/lb | Verified quote |
DOE bandwidth study, current typical on-site energy intensity of packaging of frozen vegetables, per lb of product (whole packaging step; the theoretical output of this model is per pack, compare with heat_typical_per_kg)Show verbatim quoteFreezing -53.5 to 586 279 279 -48.6 12.1 5.8 5.8 -1.02 Packaging 15 14 14 0Bandwidth Study on Energy Use and Potential Energy Savings Opportunities in U.S. Food and Beverage Manufacturing (opens in a new tab). U.S. Department of Energy, Office of Energy Efficiency and Renewable Energy, Advanced Manufacturing Office, 2017. p. 56. DOE/EE-1571; OSTI ID 1512366 | Typical | 15 Btu/lb | Verified quote |
9Unavoidable stops
- Reel change and splice (scenario stop with a manual splicer: availability_scenario only)Declared assumption
A reel holds a finite film length; at the web speed of the machine it runs out after L_r / v. A manual splice stops the machine for t_sp; an automatic zero-speed splicer removes the stop but not the splice waste.
- Format or product changeover (scenario stop: availability_scenario only)Declared assumption
Change of bag size, film or product requires stopping, adjusting forming set and jaws, and restarting with start-up waste. Declared scenario values.
10Assumptions
- No stop is forced by physics or regulation: an automatic zero-speed splicer removes the reel-change stop (the splice waste remains in the film yield) and changeovers follow the product mix, so availability_max = 1 and both stops enter only availability_scenario and oee_scenario. No cleaning-in-place applies to a form-fill-seal machine, so the cleaning model is not used. Dwell and rate with the capability margin use declared tolerances and are reported without the bat label.
- One-dimensional transient conduction through two identical film layers between two jaws at the same constant temperature (symmetric plane wall with fixed surface temperature, ideal contact).
- Constant properties evaluated near room temperature; the latent heat of fusion is not included in the conduction problem, which makes the computed dwell a lower bound, and it is included in the energy balance.
- A seal is sound when the interface reaches the sealing temperature during the dwell; under-seals and over-seals are the only quality losses (contamination of the seal area by product is not modelled).
- Film and jaw carriage move with bang-bang (triangular velocity) profiles at their maximum acceleration; the longitudinal seal does not limit the rate.
- Film yield counts splice and start-up waste only; trim does not exist in a fin-sealed pillow bag.
11Range of validity
- Polyolefin sealant films sealed with constant-temperature (hot) jaws on both sides; impulse and ultrasonic sealing are outside the model.
- Sealing temperatures below the equilibrium melting temperature of polyethylene (414.6 K) and film thicknesses of 20 to 100 micrometres per layer.
12Sensitivity
- Thickness of one film layer (distance from the jaw face to the seal interface)elasticity -0.028Spearman ρ -0.72
- Capability margin in standard deviations used to set the capable dwellelasticity -0.018Spearman ρ -0.21
- Molar mass of the CH2 repeat unitelasticity +0.014Spearman ρ —
- Thermal conductivity of the polyethylene filmelasticity +0.014Spearman ρ +0.29
- Jaw set-point above the sealing temperatureelasticity +0.011Spearman ρ +0.28
- Coefficient of variation of the film thicknesselasticity -0.010Spearman ρ -0.36
- Heat capacity of amorphous polyethylene at 310 K, per mole of CH2 repeat unit (recommended data)elasticity -0.009Spearman ρ —
- Density of amorphous polyethylene at 298 Kelasticity -0.008Spearman ρ —
- Standard deviation of the jaw face temperature under controlelasticity -0.008Spearman ρ -0.24
- Density of crystalline polyethylene at 298 Kelasticity -0.006Spearman ρ —
- Heat capacity of crystalline polyethylene at 310 K, per mole of CH2 repeat unit (recommended data)elasticity -0.005Spearman ρ —
- Film length per bag (index length)elasticity +0.004Spearman ρ —
- Maximum acceleration of the film transport (limited by film tension and slip of the pull belts)elasticity -0.004Spearman ρ -0.19
- Interface temperature required for a sound seal (seal initiation temperature of the sealant)elasticity -0.004Spearman ρ -0.03
- Maximum acceleration of the jaw carriageelasticity -0.003Spearman ρ -0.13
- Opening stroke of each jawelasticity +0.003Spearman ρ —
- Mass-fraction crystallinity of the polyethylene sealant filmelasticity +0.001Spearman ρ +0.01
- Initial film temperatureelasticity +0.001Spearman ρ +0.02
- Output rises with the parameter
- Output falls with the parameter
13Validation checks
- Dimensional analysis31 outputs converted to their declared unitsPassed
- Every cited value verified against its source8 verified, 0 failedPassed
- No documented value beats the theoretical limitPassed
- Ceilings in physical orderPassed
- Fractions within 0 and 1Passed
14Causes of loss in this operation
- Packaging machine breakdownEquipment failure (breakdowns)4.4% [1.9–8.4%]A112 studies
- Unspecified packaging defectProcess defects (scrap and rework)1.6% [0.5–3.7%]B112 studies
- 1.6% [0.5–3.6%]C112 studies
- Unspecified packaging line lossnot classifiable1.4% [0.4–3.2%]C112 studies
- Flexible package seal/forming defectProcess defects (scrap and rework)1.3% [0.4–3.0%]C112 studies
- Basic Condition and Operating Standard Non-ComplianceEquipment failure (breakdowns)1.1% [0.3–2.7%]C112 studies
- Packaging Equipment Setup and AdjustmentSetup and adjustments1.0% [0.3–2.5%]C112 studies
- Packaging line changeoverSetup and adjustments1.0% [0.3–2.3%]C112 studies
- Packing line starvation/blocking due to upstream or downstream imbalanceorganizational external0.8% [0.2–2.0%]C112 studies
- Heat seal defect (detached, wrinkled or folded seal)Process defects (scrap and rework)0.8% [0.2–2.1%]C112 studies
- Unfilled pouch (empty pouch defect)Process defects (scrap and rework)0.8% [0.2–2.0%]C112 studies
- Packaging/filling seal and handling mechanism faultIdling and minor stops (micro-stops)0.8% [0.2–2.0%]C112 studies
- Film handling and wrapping system failureEquipment failure (breakdowns)0.8% [0.2–1.9%]C112 studies
- Tray-forming clamp/finger mechanism faultEquipment failure (breakdowns)0.7% [0.2–1.9%]C112 studies
- Palletizer minor stoppage (misalignment, jam or blockage)Idling and minor stops (micro-stops)0.7% [0.2–1.8%]C112 studies
- Operator-limited line speedReduced speed0.7% [0.1–1.8%]D112 studies
- Packer guide rail adjustmentSetup and adjustments0.7% [0.2–1.8%]C112 studies
- Wrapping machine component failureEquipment failure (breakdowns)0.6% [0.1–1.6%]D112 studies
- Unplanned corrective maintenance stopEquipment failure (breakdowns)0.6% [0.1–1.6%]D112 studies
- Timing belt misalignment or failureEquipment failure (breakdowns)0.6% [0.1–1.6%]D112 studies
- Overheating-induced failure of sealing control components (scale, RCU, thermocouple)Equipment failure (breakdowns)0.6% [0.1–1.6%]D112 studies
- Perforation blade wear, breakage or foulingEquipment failure (breakdowns)0.6% [0.1–1.5%]D112 studies
- Case packer / cartoner equipment failureEquipment failure (breakdowns)0.6% [0.1–1.5%]D112 studies
- Conveyor belt system failureEquipment failure (breakdowns)0.6% [0.1–1.6%]D112 studies
- Film cutter/sealer blade failureEquipment failure (breakdowns)0.6% [0.1–1.6%]D112 studies
- Tray Corner Ear Flare DefectEquipment failure (breakdowns)0.6% [0.1–1.6%]D112 studies
- Operator execution error during packaging operationnot classifiable0.6% [0.1–1.6%]D112 studies
- Operator unavailability due to labor shortage or scheduled breaksorganizational external0.6% [0.1–1.6%]D112 studies
- Wrap/pack quality defect requiring reworkProcess defects (scrap and rework)0.6% [0.1–1.5%]D112 studies
- Aluminum foil tearingProcess defects (scrap and rework)0.6% [0.1–1.6%]D112 studies
- Carton Erector Equipment FailureEquipment failure (breakdowns)0.6% [0.1–1.5%]D112 studies
- Package fill weight deviation (variation/overfilling)Process defects (scrap and rework)0.6% [0.1–1.6%]D112 studies
- Packaging machine seal defects from component wearProcess defects (scrap and rework)0.6% [0.1–1.5%]D112 studies
- Manual non-value-added tasksnot classifiable0.6% [0.1–1.6%]D112 studies
- Unspecified palletizer lossesnot classifiable0.6% [0.1–1.6%]D112 studies
- Out-of-spec productProcess defects (scrap and rework)0.6% [0.1–1.5%]D112 studies
- Strapping machine malfunction / minor stoppageIdling and minor stops (micro-stops)0.5% [0.1–1.5%]D112 studies
- Fallen Product Requiring CleanupIdling and minor stops (micro-stops)0.5% [0.1–1.5%]D112 studies
- Pull/feed roller jamIdling and minor stops (micro-stops)0.5% [0.1–1.5%]D112 studies
- Final Folder Jam/StoppageIdling and minor stops (micro-stops)0.5% [0.1–1.5%]D112 studies
- Packaging line jam or blockageIdling and minor stops (micro-stops)0.5% [0.1–1.5%]D112 studies
- WIP and packing material adjustmentSetup and adjustments0.5% [0.1–1.4%]D112 studies
- Shift start/end line setupSetup and adjustments0.5% [0.1–1.4%]D112 studies
- Changeover material staging and organizationSetup and adjustments0.5% [0.1–1.4%]D112 studies
- Changeover adjustment of guide rails and air-blower positioningSetup and adjustments0.5% [0.1–1.4%]D112 studies
- Cardboard cutout feeding module fine-tuning stoppagesSetup and adjustments0.5% [0.1–1.4%]D112 studies
- Film and film-holding equipment changeoverSetup and adjustments0.5% [0.1–1.4%]D112 studies
- Fallen-bottle detection sensor adjustmentSetup and adjustments0.5% [0.1–1.4%]D112 studies
- Packaging program change and parameter recalculationSetup and adjustments0.5% [0.1–1.3%]D112 studies
- Product damage during restart after maintenanceStart-up losses (reduced yield)0.5% [0.1–1.4%]D112 studies
- Cutting blade failureEquipment failure (breakdowns)0.4% [0.1–1.1%]D112 studies
- Unspecified case packer lossnot classifiable0.4% [0.1–1.2%]D112 studies
- Missing or illegible expiry date printProcess defects (scrap and rework)0.4% [0.1–1.1%]D112 studies
- Excess air entrapped in sealed bagProcess defects (scrap and rework)0.4% [0.1–1.2%]D112 studies
- Defective packaging bagsProcess defects (scrap and rework)0.4% [0.1–1.2%]D112 studies
- Underfill (low fill weight/volume)Process defects (scrap and rework)0.4% [0.1–1.1%]D112 studies
- Aseptic carton form-fill-seal defectProcess defects (scrap and rework)0.4% [0.1–1.1%]D112 studies
- Bag re-feeding after misfeed or jamIdling and minor stops (micro-stops)0.4% [0.1–1.2%]D112 studies
- Improper bag attachment to filling/packaging spoutIdling and minor stops (micro-stops)0.4% [0.1–1.1%]D112 studies
- Folding bracket assembly during changeoverSetup and adjustments0.3% [0.1–1.0%]D112 studies
- Transport System Changeover AdjustmentSetup and adjustments0.3% [0.1–1.0%]D112 studies
15References
- Heat capacity and other thermodynamic properties of linear macromolecules. II. Polyethylene (Gaur, U.; Wunderlich, B.), Journal of Physical and Chemical Reference Data 10, 119 (1981) (opens in a new tab). American Institute of Physics for the National Institute of Standards and Technology (NIST reprint), 1981. p. 5. doi:10.1063/1.555636
- Bandwidth Study on Energy Use and Potential Energy Savings Opportunities in U.S. Food and Beverage Manufacturing (opens in a new tab). U.S. Department of Energy, Office of Energy Efficiency and Renewable Energy, Advanced Manufacturing Office, 2017. p. 56. DOE/EE-1571; OSTI ID 1512366
- doi:10.1063/1.555636 — Heat capacity, heat of fusion and densities of polyethylene.